Title:
コンクリート及びその製造方法
Document Type and Number:
Japanese Patent JP5828813
Kind Code:
B2
Abstract:
PROBLEM TO BE SOLVED: To attain both effective utilization of industrial and trade wastes and suppression of deterioration of durability of the same.SOLUTION: In the example Grain 0.6, steel making slag having an immersion expansion ratio not less than 1% and not larger than 20% is used as a fine aggregate passing a sieve of 0.6 mm in sieving according to JIS A 1102 in one example of concrete. Popout does not occur in specimen (Plain Concrete) and Grain n (n=0.6, 0.3) in which the steel making slag is not used and only natural aggregate is used as the fine aggregate, popout occurs in grain n (n=5.0, 2.5, 1.2). The adding quantity of AE water reducing agent is substantially the same in the grain n (n=0.6, 0.3) and the Plain Concrete.

Inventors:
Takeshi Yamada
Hiroaki Tsuruta
Application Number:
JP2012182692A
Publication Date:
December 09, 2015
Filing Date:
August 21, 2012
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
KABUSHIKI KAISHA KOBE SEIKO SHO
Kansai University
International Classes:
C04B28/02; C04B18/14; C04B20/00
Domestic Patent References:
JP50092316A
JP2005247627A
JP2001019529A
JP2004292295A
JP2003293345A
JP2005281087A
JP2002104849A
Attorney, Agent or Firm:
Yoshiyuki Kaji
Makoto Suhara