Abstract:

To provide a composite ceramic having excellent wear resistance in addition to high strengths and high toughness and a method for manufacturing the same.

In the composite ceramic constituted of a zirconia crystal phase 1 containing 2.8-4.5 mol% Y2O3and a metallic phase 3 composed of one of Mo and W or a mixture of Mo with W, the average particle diameter of the zirconia crystal phase 1 is ≤0.35 μm, the average particle diameter of the metallic phase 3 is ≤1 μm, the content of the metallic phase 3 in the composite ceramic is 5-25 mass% and ≥95% of metallic phase 3 exists in the grain boundary of the zirconia crystal phase 1.

COPYRIGHT: (C)2005,JPO&NCIPI


Inventors:
Kunihide Shikata
Application Number:
JP2003151143A
Publication Date:
March 25, 2009
Filing Date:
May 28, 2003
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Kyocera Corporation
International Classes:
C04B35/48; B22F3/10; B22F3/15; C22C1/05; C22C29/12
Domestic Patent References:
JP6172026A