Abstract:

PURPOSE: To form flat BaCoxTixFe12-2xO19 particle for magnetic recording and improve its characteristics by a method wherein the ratio of Ba ion to Fe(III), Co(II) and Ti(IV), the density of an alkaline solvent, the reaction temperature and time, the stirring condition of a suspension and the like are varied to obtain the prescribed production condition.

CONSTITUTION: The ratio of the total number of atoms of Co(II) and Ti(IV) is 0.17W0.09 to one atom of Fe(III). A high alkaline suspension, in which the number of atoms of contained Ba ion is one to 7W9 atoms of Fe, Co and Ti metal ions, is subjected to hydro-heat treatment at the temperature range of 250W 320°C. BaCoxTixFe12-2xO19 (where 0.1≤x≤0.5) fine particle, whose BEF rational surface area is 20W70m2g-1, average diameter is 0.05W0.3μm, magnetization value under the magnetic field of 10kOe is more than 30enug-1 and coercive force is 300W1,000Oe, is produced from the solution. This fine particle is used as flat Ba-ferrite fine particle for magnetic recording.


Inventors:
NAGAI NORIMICHI (JP)
HORIISHI NANAO (JP)
KIYAMA MASAO (JP)
TAKADA TOSHIO (JP)
Application Number:
JP5080083A
Publication Date:
October 04, 1984
Filing Date:
March 26, 1983
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
TODA KOGYO CORP (JP)
SEISAN KAIHATSU KAGAKU KENKYUS
International Classes:
G11B5/62; C01G49/00; G11B5/706; H01F1/11; (IPC1-7): C01G49/02; G11B5/70; H01F1/11
Domestic Patent References:
JPS57212623A1982-12-27