JPH10237249A
To provide a vinyl chloride plastisol composition which can form a coating film capable of revealing good chipping resistance and sufficient soundproof performance even with a single-layer structure. This composition comprises mainly a v...  
JPH10237309A
To obtain the subject binder not separating a thermoplastic elastomer, even when stored at a high temperature, and capable of holding a uniform state over a long period by compounding asphalt, the thermoplastic elastomer and carbon black...  
JPH10509193A
Bitumen compositions comprising bitumen and at least one succinic anhydride derivative contained in the bitumen, processes for their preparation and their use in bitumen emulsions for road applications, e.g. surface dressings.  
JP2794012B2
PURPOSE:To form an asphalt modifier with a large grasping force and adhesive force to an aggregate, soluble in an asphalt in a short time and with good long-term stability by emulsifying and dispersing a thermoplastic elastomer in the pr...  
JP2787753B2  
JP2787755B2  
JPH10219118A
To provide a dissolution treatment liq. for polystyrene and asphalt which enables a hot-asphalt waterproofing to be repaired safely without needing skill and without causing an odor problem and which enables the effective utilization of ...  
JPH10219117A
To provide a novel asphalt improver which is excellent in performance and solubility or dispersibility in asphalt and can be granulated and an improved asphalt compsn. which is prepd. therefrom and has high toughness, tenacity, and elong...  
JPH10195301A
To obtain a binder which undergoes less separation of a constituent thermoplastic elastomer and can be kept in an uniform state for a long time even when stored at high temperatures by uniformly mixing the thermoplastic elastomer with ca...  
JPH10195300A
To obtain the subject grouting material comprising a specific cement, an anticracking material, a water-reducing agent, a coloring material and glass powder in a specific ratio, and capable of preventing the deterioration in the visibili...  
JPH10182982A
To provide an asphalt-epoxy resin composition that can retain resistances to wearing, fluidity and load, has improved workability due to its prolonged pot life and is improved in its flexibility at low temperature, as for asphalt for pav...  
JPH10182983A
To obtain an aqueous binder that can bond a base material at room temperature and impart excellent storability, handleability, energy saving and environmental suitability to asphalt for pavement by using a water-soluble epoxy compound an...  
JP2769361B2  
JPH10169385A
To improve the progress of work by an accelerating hardening spray rubber asphalt having a rapid curing speed. An agent A composed of a rubber asphalt emulsion as a chief agent and a cement powdery material mixed with the emulsion and an...  
JPH10147717A
To provide an easily handleable asphalt emulsion suitable for paving of a road, thin-layer paving, roofing, flooring, etc. This emulsion comprises (I) 100 pts.wt. asphalt, (III) 5 to 100 pts.wt. block copolymer composed of (C) a block co...  
JPH10140164A
To obtain an improved asphalt compsn. which, when used as a pavement binder, imparts excellent resistances to flow and fatigue to a pavement by reacting sulfur with petroleum asphalt and then with an unsatd. hydrocarbon. Pref. petroleum ...  
JPH10139983A
To provide a curable composition, which can give a cured product having flexibility, abrasion resistance, oil resistance and waterproofness and is useful as a protective coating material, and to provide a cured product thereof. This comp...  
JP2755240B2
To obtain the subject composition excellent in flame retardancy, free from generation of any toxic gas in case of a fire or in incineration disposal thereof, low in environmental load with safely, thus useful for e.g. electronic parts, c...  
JPH10130509A
To obtain a vibration damper having an excellent vibration-damping properties at a high temperature range and light weight, and capable of exhibiting moderate flexibility, useful for vibration damping of vehicles, etc., by incorporating ...  
JP2748970B2
To prevent the clogging of a device and manufacture foamed asphalt which is uniform and of high quality by a method wherein a flow control valve and a nozzle part are provided, and water and compressed air are blown against heated asphal...  
JP2749544B2
To provide a captioned emulsion which is stabilized by use of a surface active agent naturally occurring in a viscous hydrocarbon and can be used as a fuel. An intended emulsion is obtained by supplying (B) a viscous hydrocarbon containi...  
JPH10119168A
To provide an easily reusable functional sheet without a release sheet, while maintaining the damping effect and the shock resistance equivalent to conventional functional sheets. In a functional sheet including a functional member and a...  
JPH10120843A
To obtain an asphalt improver which has an excellent solubility in asphalt and, when compounded with asphalt, gives a compsn. improved in strength of adhesion to an aggregate by using, as the improver, a specific ethylene copolymer produ...  
JPH10120839A
To provide an asphalt improver excellent in solubility in asphalt and to provide an asphalt compsn. contg. the same. This asphalt improver contains an ethylene copolymer which comprises repeating units derived from ethylene and repeating...  
JP2748037B2
PURPOSE:To prepare an asphalt emulsifier of which the decomposition time during application is widely adjustable by neutralizing a specific diamine and a specific quaternary ammonium chloride with phosphoric acid. CONSTITUTION:A diamine ...  
JPH1094772A
To provide a treating method of a waste for giving a final product having small quantity of soluble fraction with a small quantity of a binder and the device. This method includes a step for homogenizing a residue R, a step for performin...  
JPH1088001A
To obtain an asphalt mixture having good characteristics while controlling the usage of asphalt by dry mixing a heated aggregate with a specified amount of a thermoplastic material and a filler, and then wet mixing this mixture with a sp...  
JPH1088000A
To obtain an asphalt mixture improved in mechanical strength, stability and applicability, and useful as a road paving material by mutually mixing aggregates, asphalt, filter, and a specific amount of thermoplastic material similar in gr...  
JP2734666B2  
JPH1081790A
To impart a water-proofing tape, which is to be fixed with nails, with corrosiono-proof function against nails and water-swelling pressure-caused water-stopping effect. This water-proofing tape essentially comprises a corrosion-proof wat...  
JPH1081828A
To obtain an asphalt for a waterproofing work which emits less smoke and odor when applied by adding a vacuum residue to an asphalt for a waterproofing work specified in JIS to produce a composition having properties specified in JIS. 85...  
JP2731442B2
Bitumen-polymer compositions are prepared, between 100 DEG C and 230 DEG C, by mixing bitumen with a copolymer of styren and a conjugated diene and a coupling agent susceptible of providing sulfur, the copolymer and the coupling agent be...  
JPH1077602A
To save resources, such as crushed stone used as an aggregate and to cope with chronic insufficiency in an asphalt aggregate by a method wherein ash discharged from a refuse incinerating yard is reheat-treated to produce molten slag, whi...  
JPH1072245A
To provide a sulfur mortar structure not only showing practically sufficient strength even when aggregate such as gravel or crushed stone is blended but also easy for production and having high bending strength and lightweight property c...  
JPH10502701A
PCT No. PCT/FR96/00159 Sec. 371 Date Dec. 13, 1996 Sec. 102(e) Date Dec. 13, 1996 PCT Filed Jan. 20, 1996 PCT Pub. No. WO96/23840 PCT Pub. Date Aug. 8, 1996The invention relates to improved bitumen compositions including: (A) 100 parts o...  
JPH1060286A
To obtain a modified asphalt composition for paving, having a large modification effect due to a modifying material, excellent in heat storage stabil ity, hardly causing rutting of pavement after construction on road, almost free from cr...  
JP2714419B2  
JP2714420B2  
JP2714418B2  
JP2714257B2
PCT No. PCT/CA93/00562 Sec. 371 Date Sep. 12, 1995 Sec. 102(e) Date Sep. 12, 1995 PCT Filed Dec. 29, 1993 PCT Pub. No. WO91/14896 PCT Pub. Date Jul. 7, 1994The present invention provides a procedure for at least partial dissociation of c...  
JP2711102B2  
JPH1036677A
To obtain a filled thermoplastic B-stage pitch preform freed from voids and cracks and having an improved bulk density by mixing a powdery filler with a mesophase pitch. 6-80wt.% powdery filler 11' is mixed with 94-20wt.% mesophase pitch...  
JPH1036450A
To obtain a starting polyacrylonitrile/pitch material for producing carbonaceous material excellent in strengths, etc., by dissolving or dispersing a pitch having a specified softening point in an electron-donating solvent and polymerizi...  
JP2707131B2  
JP2706754B2
PURPOSE: To obtain a modifying agent consisting of an oil soluble polymer containing an acidic group and an oil soluble polymer containing a basic group, having good dissolution in an asphalt, flow property and dispersibility, and capabl...  
JP2707132B2  
JP2702956B2
Dispersions of hydrophobic substance eg resin emulsions, usually having a relatively low average particle size can be continuously and speedily prepared by feed a hydrophobic substance in the liquid state into at least two static mixers,...  
JP2700806B2  
JPH1017777A
To obtain an asphalt composition causing little separation of an elastomer even by storing at a high temperature, keeping the uniform state over a long period and suitable for the pavement of street by compounding an asphalt with a therm...  