To enhance not only heat resistance and chemical resistance but also dynamic properties and dimensional stability of a long fiber nonwoven fabric made of a core/sheath fiber using a polyarylene sulfide as a sheath component.
The long fiber nonwoven fabric uses a composite long fiber consisting of a sheath component containing not less than 95 pts.mass polyarylene sulfide and a core component containing a thermoplastic resin satisfying the relationship of TmcTmsTmc+30C between a melting point Tmc (C) of the core component and a melting point Tms (C) of the sheath component and the relationship of TgcTgsTgc+30C between a glass transition point Tgs (C) of the sheath component and a glass transition point Tgc (C) of the core component in a weight ratio of the core component to the sheath component of 40-60 to 60-40 and is formed by integrating the composite long fibers by bonding, wherein the strength of a single fiber in the composite long fiber is not less than 3.0 cN/dtex and the dry heat shrinkage percentage at 180C (SHD180) of the single fiber is not more than 10%.
INATOMI SHINICHIRO
ISODA HIDEO
JPH0340813A | 1991-02-21 | |||
JPH0299614A | 1990-04-11 | |||
JPS59204920A | 1984-11-20 | |||
JPH10174822A | 1998-06-30 | |||
JPS63126956A | 1988-05-30 | |||
JPS5831112A | 1983-02-23 | |||
JPH0959841A | 1997-03-04 | |||
JP2005171415A | 2005-06-30 | |||
JP2007152216A | 2007-06-21 | |||
JP2007513270A | 2007-05-24 | |||
JP2002180366A | 2002-06-26 | |||
JPH08158232A | 1996-06-18 | |||
JP2006274512A | 2006-10-12 | |||
JP2007023444A | 2007-02-01 |
JPN6012065754; プラスチック材料活用事典 編集委員会: プラスチック材料活用事典 初版第1刷, 20011020, 第677,679頁, 産業調査会 事典出版センター
Noriko Asano
Next Patent: LOW-DUSTING CONDUCTIVE YARN AND PROCESS FOR PRODUCING THE SAME