PURPOSE: To produce an amorphous material having high quality at a high yield by ejecting a molten metal from a nozzle in the direction near the tangent in the rotating direction of a high speed rotating roll and cooling and solidifying quickly the metal to a tape and ejecting high pressure gas to the tape.
CONSTITUTION: The ejecting direction (a) of a molten metal 8 from a nozzle 7 is set in the tangent direction (c) of a high speed rotating roll 6 or the angle θ thereto is set at about 0W20° in a method for obtaining an amorphous tape 10 by rotating the roll 6 in an arrow (b) direction, ejecting the molten metal 8 from the nozzle 7 toward the same and solidifying instantaneously the metal. Inert gas 11 maintained under a high pressure is ejected from an auxiliary ring 9 provided along the gap α at a prescribed distance from the outside circumference of the roll 6 to the surface of the tape 10 on the side opposite from the roll 6 so that the long contact time between the roll 6 and the tape 10 is maintained. The above-mentioned gap α is preferably set at about ≤0.1mm, the length of the ring 9 at about 1/4 of the circumfernce the roll 6 and the width of the gaseous flow to be ejected about twice the width of the tape 10.
YAMAGUCHI MASARU
MOURI SHIYOUICHI
SUMIYA SHIGERU
JPS5741850A | 1982-03-09 | |||
JPS55109547A | 1980-08-23 | |||
JP57111448B |