Document |
Document Title |
JP2017534460A |
Laser cladding mechanical face seal A method of manufacturing a mechanical face seal that includes the acquisition step of a cast or forged substrate (400) having an inner diameter, an outer diameter and a planar surface (440). The metho...
|
JP2017192964A |
To provide an insert member in which a core inserted when casting a cast part can be easily pulled out, and a method for manufacturing the insert member.One end side of a cylindrical pipe part 25 is inserted thereby forming a cast part 2...
|
JP2017192965A |
To provide an insert member in which a core inserted when casting a cast part can be easily pulled out, and a method for manufacturing the insert member.An interior of a pipe part 25 on one end side is covered thereby forming an inner co...
|
JP2017185545A |
To elongate sensitive hollow blocks or tubes in a hot-forming elongator while maintaining, if possible, the internal structure that is present or that forms immediately after casting, thereby making it possible that, in the case of suita...
|
JP6201074B1 |
[Subject] A lining steel pipe created on Casting -basis by centrifugal casting is provided. [Means for Solution] Lining steel pipe 1 which is a double steel pipe of a different-species material created by Casting -basis has steel pipe 10...
|
JP2017148844A |
To provide a method for production of a TiAl-based alloy member having an included ductile material in a final product using a melting and casting method more considerably convenient than a powder sintering method and having high dimensi...
|
JP2017139462A |
To provide a water cooling circuit board which achieves good mass productivity and low costs and causes no problems of coolant leakage, and to provide a manufacturing method of the water cooling circuit board.A water cooling circuit boar...
|
JP6169858B2 |
Casting preforms (120) are provided comprising a casting preform assembly (130); and a plurality of geometrically shaped bodies (140), wherein the plurality of geometrically shaped bodies (140) are arranged or interconnected to form the ...
|
JP6161665B2 |
|
JP6149229B2 |
|
JP2017104907A |
To provide an insert casting member manufactured by casting, which is an insert casting member manufacturable easily and inexpensively, and capable of securing bond strength between a material to be insert-cast and an insert casting mate...
|
JP6147265B2 |
A method for producing a metal part, the part including, in particular, a first set of elements having a small thickness, and a second set of elements having a large thickness, the method including: forming a peripheral portion of the el...
|
JP6148385B2 |
The aluminum structure member according to the present invention is provided with an aluminum wrought material comprising aluminum or aluminum alloy, and an aluminum alloy casting joined in a state in which the aluminum wrought material ...
|
JPWO2016002943A1 |
To suppress damage such as cracks and cracks in a through hole and a peripheral portion thereof generated when fixing a heat radiating component to another component or in actual use after fixing, and to prevent a shrinkage or a hole dur...
|
JP2017101561A |
To provide a manufacturing method of a closed deck type cylinder block capable of preventing a gap between a hollow member and a cylinder liner from being excessively increased.An intermediate member 4 is held between a cylinder liner 2 ...
|
JP2017087232A |
To provide a composite material which prevents a wear-resistant material integrated with a base material surface from peeling, and is inexpensive and is easy to manufacture.A material cost of a wear-resistant material 2 can be suppressed...
|
JP2017512138A |
A method of forming a composite component from a plurality of feed materials by heating is disclosed. A negative ceramic mold (102) is obtained that defines the shape of the component formed. First, a first feed material (104) and a seco...
|
JP6117619B2 |
|
JP6118949B2 |
A cylinder liner for an internal combustion engine may include an aluminum alloy material including a magnesium content of at least 0.3% by weight, a liner body having a circumferential face, and an adapter layer of silicon oxide dispose...
|
JP6117428B2 |
|
JP6117427B2 |
|
JP6117575B2 |
|
JP6116450B2 |
|
JP6109101B2 |
The invention relates to a method for manufacturing a metal-ceramic composite structure (20) intended to be exposed to high temperatures, comprising a base metal structure or component (19), which is on at least one side covered and perm...
|
JP6110012B2 |
The present invention provides piston production device and piston production method capable of surely holding friction-resistant ring regardless of presence or absence of decrease in accuracy of outside diameter of holding pin. Device h...
|
JP6087366B2 |
A centrifugal casting apparatus including: a lower half-mold (10) mounted on a support (12) provided with driver for rotation about a substantially vertical central axis (14), the lower half-mold (10) being a solid of revolution having a...
|
JP2017039997A |
To provide an aluminum alloy-ceramic composite material having a modulus of longitudinal elasticity adjusted in a predetermined range while having strength equal to or more than conventional ones, and a production method enabling such al...
|
JPWO2015002289A1 |
To provide a rotating body shaft, rotating body structure and wheels with sufficient torsional strength while keeping costs low. The rotating body shaft 3 having a plurality of protrusions on the outer peripheral surface in a cast materi...
|
JP2017504482A |
Incorporating hard particles into the matrix to form the surface of the member can significantly increase wear resistance. The carbon structure is decomposed into graphite in air at temperatures above 700 ° C, limiting the practical use...
|
JP2017024029A |
To provide a different material structural member that can joint an aluminum material to a steel material at high-mechanical strength and readily connected to other members.The different material structural member 100 includes: the alumi...
|
JP2017019241A |
To provide an injection molding system in which an insert product can be accurately inserted with a simple structure.An injection molding system comprises: a mirror surface member for reflecting an insert product which is held by insert ...
|
JP6067386B2 |
A method for manufacturing a boron-containing aluminum plate material comprises: a spreading step for spreading boron-containing alloy particles (3) in the shape of a layer over a bottom plate (2) placed in a container (1); a preheating ...
|
JP6064120B2 |
|
JP6044737B2 |
A molding machine cylinder comprising a lining layer having a structure comprising 20-50% by area of tungsten carbide particles and 1-10% by area of tungsten-based metal carboboride particles in a nickel-based alloy matrix, and containin...
|
JP2016199459A |
To provide a method for producing a metal-ceramics composite material, in which even when the metal-ceramics composite material has a comparatively thick product shape, a void can be restrained from being formed on the inside of a produc...
|
JP6036275B2 |
|
JP6034034B2 |
|
JP6033782B2 |
A metal filling apparatus fills molten metal into a minute space formed on a surface of a semiconductor wafer. The apparatus has a processor body with a chamber in which the wafer is held, a molten metal supply, and a molten metal recove...
|
JP6036698B2 |
A centrifugally cast composite roll for hot rolling comprising an outer layer having a composition comprising by mass 0.8-3.5% of C, 0.1-2.5% of Si, 0.1-2.5% of Mn, 1.2-15% of Cr, 1-5% of Ni, and 1-10% of Mo + 0.5 x W, the balance being ...
|
JP2016196039A |
To provide a method of producing a compound steel plate having both properties of ceramic and tungsten by using brown gas.Tungsten is fused in brown gas with ceramic at the high temperature to make a uniform composition and then to gradu...
|
JP6030507B2 |
|
JP6026721B2 |
A composite cast tool is cast in one continuous piece, partly of steel and partly of grey iron, so that an interconnection zone is formed between the steel and the grey iron. The steel portion forms the working component of the tool, for...
|
JP6022626B2 |
|
JP2016180185A |
To provide a production method of an aluminum alloy-ceramic composite, enabling the aluminum alloy-ceramic composite excellent in crack resistance and peeling resistance to be efficiently produced.According to the invention, the producti...
|
JP6007840B2 |
|
JP6003839B2 |
|
JP6004314B2 |
|
JP2016172329A |
To provide a die for molding correctly arranged with a molded component with a three-dimensional shape having deviation in weight and further capable of swiftly performing injection molding such as insert treatment.Provided is a die for ...
|
JP5998637B2 |
|
JP5988667B2 |
|